Product Details
Place of Origin: Zhengzhou ,China
Brand Name: Rongsheng Xinwei
Certification: ISO9001
Model Number: Magnesia iron Spinel Brick, High toughness Magnesium Iron Spinel brick
Document: Product Brochure PDF
Payment & Shipping Terms
Minimum Order Quantity: 1 Ton
Price: 200-800USD
Packaging Details: packed on wooden pallets, with water-proof cover, and tightened with plastic/steel bandages
Delivery Time: 20-30DAYS
Payment Terms: TT; L/C
Supply Ability: 2000tons /month
Application Temperature: |
≤1450℃ |
Chemical Composition: |
MgO≥90% |
Color: |
White |
Compressive Strength: |
≥50MPa |
Density: |
2.9-3.2g/cm3 |
Linear Change Rate: |
≤0.2% |
Material: |
Magnesite |
Package: |
Wooden Pallet |
Porosity: |
≤20% |
Refractoriness: |
≥1700℃ |
Refractoriness Under Load: |
≥1450℃ |
Shape: |
Bricks |
Size: |
Standard |
Thermal Conductivity: |
Low |
Thermal Shock Resistance: |
Good |
Application Temperature: |
≤1450℃ |
Chemical Composition: |
MgO≥90% |
Color: |
White |
Compressive Strength: |
≥50MPa |
Density: |
2.9-3.2g/cm3 |
Linear Change Rate: |
≤0.2% |
Material: |
Magnesite |
Package: |
Wooden Pallet |
Porosity: |
≤20% |
Refractoriness: |
≥1700℃ |
Refractoriness Under Load: |
≥1450℃ |
Shape: |
Bricks |
Size: |
Standard |
Thermal Conductivity: |
Low |
Thermal Shock Resistance: |
Good |
Magnesia Iron Spinel Brick For Cement Rotary Kiln Furnace
Introduction of magnesia iron spinel brick
Magnesia iron spinel bricks are a type of refractory material commonly used in high-temperature industrial applications. They are made from a combination of magnesia and iron oxide, which forms a unique crystal structure known as spinel. This composition provides the bricks with excellent thermal, chemical, and mechanical properties, making them suitable for various industrial processes.
Features of Magnesia iron spinel brick
Magnesia-iron spinel bricks have high thermomechanical properties and thermochemical properties in addition to the excellent kiln skin properties of magnesia-chrome bricks
Item | Index | |
Magnesia iron Spinel Brick | High toughness Magnesium Iron Spinel brick | |
MgO % | ≥85 | ≥88 |
Fe2O3 % | 5~7.5 | 5~6 |
Al2O3 % | 3~5 | 4~7 |
Bulk density g/cm3 | ≥3 | ≥2.9 |
Apparent porosity % | ≤17 | ≤16 |
Cold Crushing Strength MPa | ≥45 | ≥55 |
Thermal shock resistance cycle 1100℃water cooling | ≥6 | ≥8 |
0.2MPa Refractoriness under load ℃ | ≥1600 | ≥1650 |
Thermal expansion rate % 1400℃ | ≤1.6 | ≤1.7 |
Thermal conductivity W/(m·K) 350±25℃ | ≤2.6 | ≤2.6 |