Product Details
Place of Origin: Zhengzhou ,China
Brand Name: Rongsheng Xinwei
Certification: ISO9001
Model Number: RS-65, RS-70, RS-75, RS-95
Document: Product Brochure PDF
Payment & Shipping Terms
Minimum Order Quantity: 1 Ton
Price: 200-800USD
Packaging Details: packed on wooden pallets, with water-proof cover, and tightened with plastic/steel bandages
Delivery Time: 20-30DAYS
Payment Terms: TT; L/C
Supply Ability: 2000tons /month
Al2O3 Content: |
≥48% |
Apparent Porosity: |
≤20% |
Bulk Density: |
≥2.2g/cm3 |
Chemical Resistance: |
Good |
Cold Crushing Strength: |
≥50MPa |
Compressive Strength: |
≥100MPa |
Linear Change Rate Of Reheating: |
≤0.2% |
Material: |
High Alumina Refractory Brick |
Moisture Content: |
≤1.0% |
Refractoriness: |
≥1790℃ |
Softening Temperature: |
≥1400℃ |
Thermal Conductivity: |
≤1.5W/m.K |
Thermal Expansion Coefficient: |
≤0.6% |
Thermal Shock Resistance: |
Good |
Shape: |
Ball |
Al2O3 Content: |
≥48% |
Apparent Porosity: |
≤20% |
Bulk Density: |
≥2.2g/cm3 |
Chemical Resistance: |
Good |
Cold Crushing Strength: |
≥50MPa |
Compressive Strength: |
≥100MPa |
Linear Change Rate Of Reheating: |
≤0.2% |
Material: |
High Alumina Refractory Brick |
Moisture Content: |
≤1.0% |
Refractoriness: |
≥1790℃ |
Softening Temperature: |
≥1400℃ |
Thermal Conductivity: |
≤1.5W/m.K |
Thermal Expansion Coefficient: |
≤0.6% |
Thermal Shock Resistance: |
Good |
Shape: |
Ball |
Description of 99% Purity Alumina Oxide Ceramic Beads Ball Refractory Ball Mill Grinding of Alumin Ceramic Balls
Product Specification of Description of 99% Purity Alumina Oxide Ceramic Beads Ball Refractory Ball Mill Grinding of Alumin Ceramic Balls
Item
|
High alumina
|
Low creep
|
Mullite
|
Corundum
|
Size(mm)
|
40-80
|
40-80
|
40-80
|
40-80
|
AL2O3(%)
|
65
|
70
|
75
|
95
|
Refractoriness under load(°C)
|
1450
|
1460
|
1530
|
1650
|
Apparent Porosity(%)
|
25
|
23
|
22
|
18
|
Bulk Density(g/cm3)
|
2.3
|
2.4
|
2.5
|
3.1
|
Cold crushing strength(Mpa)
|
13
|
14
|
32
|
36
|
Thermal shock resistance
(1100°Cwater cooling) cycle ≥ |
15
|
10
|
20
|
7
|
Refractoriness(°C)
|
1710
|
1750
|
1800
|
1800
|