SiO2 Content: |
88%-91% |
Chemical Resistance: |
Excellent |
Color: |
Light Yellow |
Compressive Strength: |
2-5MPa |
Durability: |
Good |
Certificate: |
ISO9001 |
Heat Resistance: |
Good |
Material: |
Ceramic |
Porosity: |
≤ 50% |
Refractoriness: |
1500~1550℃ |
Shape: |
Rectangular |
Thermal Conductivity: |
0.2-0.3W/mK |
Thermal Stability: |
≥1000℃ |
Thickness: |
50mm |
Usage: |
Lining Material |
SiO2 Content: |
88%-91% |
Chemical Resistance: |
Excellent |
Color: |
Light Yellow |
Compressive Strength: |
2-5MPa |
Durability: |
Good |
Certificate: |
ISO9001 |
Heat Resistance: |
Good |
Material: |
Ceramic |
Porosity: |
≤ 50% |
Refractoriness: |
1500~1550℃ |
Shape: |
Rectangular |
Thermal Conductivity: |
0.2-0.3W/mK |
Thermal Stability: |
≥1000℃ |
Thickness: |
50mm |
Usage: |
Lining Material |
Product Description of Lightweight Silica Insulation Bricks For Superior Thermal Insulation in High-Temperature Environments
Silica Insulation Bricks
|
|||||
Item/Index
|
RS-0.8
|
RS-1.0
|
RS-1.1
|
RS-1.15
|
RS-1.2
|
SiO2 %
|
≥88
|
≥91
|
≥91
|
≥91
|
≥91
|
Bulk Density g/cm3
|
≤0.85
|
≤1.00
|
≤1.10
|
≤1.15
|
≤1.20
|
Cold Crushing Strength Mpa
|
≥1.0
|
≥2.0
|
≥3.0
|
≥5.0
|
≥5.0
|
Thermal Conductivity (W/MK) 350℃
|
0.55
|
0.55
|
0.60
|
0.65
|
0.70
|
Permanent Linear Change On Reheating (%) 1450℃*2h
|
0~+0.5
|
0~+0.5
|
0~+0.5
|
0~+0.5
|
0~+0.5
|
0.2Mpa Refractoriness Under Load T0.6℃
|
≥1400
|
≥1420
|
≥1460
|
≥1500
|
≥1520
|
20~1000℃ Thermal Expansion 10.6/℃
|
1.3
|
1.3
|
1.3
|
1.3
|
1.3
|
Production Process of Lightweight Silica Insulation Bricks
Put raw materials and water into a kneading equipment according to a certain proportion and then kneaded into mud. Shape the mud into bricks through molding by machine or manpower. Then dry the bricks till the residual water content is lower than 0.5%, which prevent the volume expansion from the crystal transformation of SiO2. At the end, fire the shaped bricks in the high temperature, but pay attention that increase and decrease the temperature slowly when firing.